Anyone know what polarity to set up the MIG machine for this wire (ESAB
7100 Ultra -inner shield plus gas). Do you use the MIG gas welding set-up or the inner shield set-up?
Thanks Steve L.
DC Electrode Positive. C25 shielding gas. That is my favorite Gas Shielded Flux Core wire.
Read the full replyAnyone know what polarity to set up the MIG machine for this wire (ESAB
Thanks Steve L.
DC Electrode Positive. C25 shielding gas.
That is my favorite Gas Shielded Flux Core wire.