small water cooled mig

Oct 30, 2004 4 Replies
Jump to replies (4)

are there any small (for tighter work clearance) water cooled mig guns available? have not found one less than 350 amps...



thnx,


I have never heard of a water cooled MIG below 350 amps.

Most MIG guns up to 400 amps are air cooled.

Why do you want a water cooled MIG gun for smaller work?

wellll, i have come into possession of a dandy chiller and was thinking about putting it to use. a smallish (ala magnum100) gun that would handle 200~300 amps seems appealing for close-up/tighter work

But the gun would never get hot enough to warrant the cooler. Put it on ebay or use it for a TIG torch.

i was thinking of one of those guns that come on the 120 volt units, tweeco indicates they are rated for 165 amps max

"

the