Welding stainless to mild steel

Apr 26, 2009 4 Replies
Jump to replies (4)

I have a child bicycle seat made so that a child can ride in a bike behind an adult. This seat has two legs made of steel, that are not long enough to properly fasten to bicycle frame neat the rear axle hub.



I would like to extend this piece and can use 304 stainless. Can I safely weld 304 to mild steel, with E308 filler rod?


The dealer told me to use 312 for mild & stainless. This is the job:

formatting link
flux fumes were irritating.

jsw

I found a way to do what I wanted, without welding. It would be a lot better in many respects. But thanks, I will remember it.

i

To weld stainless to carbon steel you can use basic 308L filler, but the welds may crack over time.

312, and 309 are better choices for dissimilar metals.

I have had good luck with 310 for general welding of 'difficult' steels. There was a time when it was quite common to use 310 ss for welding tip shanks on heavy digging buckets as it gave good life under high impact loading.

Good luck, YMMV