Hi Can someone give me phase diagram of Ni-based superalloy Inconel 625.



Nauman



You should look for Fe-Ni-Co ternary phase diagram in ASM handbook.

snipped-for-privacy@gmail.com wrote:

One option would be to contact Computational Thermodynamics Inc., a US-based consulting company specialized in phase-diagram calculations. The company uses Thermo-Calc, coupled with specialized commercial thermodynamic databases. The Company's URL is

formatting link
and its e-mail address is snipped-for-privacy@calphad.com.

Dr. K.