It is 2" in size.
Made a Turner's cube
Mar 19, 2011
37 Replies
formatting link
formatting link
That is really, really cool. I also like the 'demo samples' the rapid prototyping guys have on their stands at exhibitions. Spheres within cubes within ellipsoids etc....
JB
formatting link
That's cute. Surely you can get out your tiny end mills and work it down a few more levels...
formatting link
>
I saw some cool examples too.
The code to do it, is actually a recursive G code function (which is understandable, since the shapes are recursively nested).
(Makes a turner's cube. See projects.txt for formulas).
O sub # = #1 (X Center) # = #2 (Y Center) # = #3 (Current Z) # = #4 (Side) # = #5 (Mill Diameter) # = #6 # = #7
# = [# * #/2]
O if [ # gt #] G0 X# Y# O call [# + 0.01] # = [ [#/2 - #] + #*#*[1 - 1/sqrt[ 2 ]]]
O call [#] [#] [# + 0.01] [# - #] [#] [#]
# = [# - 2*#]
O call [#] [#] [# - #] [#] [#] [#] [#] O endif
G0 X# Y# O call [# + 0.01] O endsub
M2
formatting link
>
That's possible, but would add to the time expense. I was thinking, to try selling this stuff on ebay.
My work involved here, is to open the vise six times and flip the cubes in the vise.
i
formatting link
> >
Dude, you have a 4th axis, only two vise changes required. Load part and machine sides 1-4, stop, flip part and machine sides 5 and 6.
formatting link
>>
It would also greatly add to the fixturing precision that is required.
i
formatting link
> > >
Add to that, probably use custom soft jaws in the small vice on the 4th axis in order to properly locate the part. Also probably machine in AL, polish in a tumbler and anodize for sale.
formatting link
formatting link
>> >
I think that clamping this is to rotary table do difficult, that flipping the part over 6 times is easier.
If I wanted to make quantities, I would machine three cubes at a time, setting three in a row in a vise.
i
formatting link
>> > >
Oh, yes, I realize that I have a question. How can I make this cube beautiful, as in, remove manufacturers marks on the aluminum,. etc?
Tumbling? In what?
i
FWIW, three is a vice is asking for trouble. One will be loose. Four in a vice - OK. multiple vices - OK.
Karl
I'm going to guess w/o reading the rest of the thread first, you did it on your mill?
You are having way too much fun :)
Wes
formatting link
> >> > >
I'd look at the large vibratory polisher / tumbler that HF sells (on sale now). It looks like it should be large enough to handle 2" cubes.
formatting link
I have the smaller version that I picked up for cleaning / polishing brass for reloading, but I haven't got around to using it yet. It looks decent enough at any rate.
formatting link
They also carry some assorted media for the tumblers, and of course you can get media from a lot of other places as well.
Polishing is the first step of course, after that you need some sort of finish to protect from rust or oxidation. There are a lot of options depending on what material you are making the parts from, look at the Caswell site for various ideas.
formatting link
> >> >
Clamping on the RT shouldn't be that difficult really.
If you want production, clearly you'll need to make a custom fixture to hold six or eight cubes, with air over hydraulic clamping, and a parts handling robot to flip the cubes around for you while you watch on the webcam from your office :)
Ignoramus4120 fired this volley in news:goqdnZfk9pS3exnQnZ2dnUVZ snipped-for-privacy@giganews.com:
Ig, it's pretty, as far as you went. But why didn't you complete it?
LLoyd
Bead blasting will give it a matte finish.
Hope This Helps! Rich
Did I say beadblast?
formatting link
Cheers! Rich
Yes, on the mill. I have a bunch of relatives visiting right now, they all decided that they want a cube like this. :)
That doesn't look anything like Huxley's brave new drug, Soma.
-- "A patriot must always be ready to defend his country against his government." --Edward Abbey
formatting link
>>>>>>
formatting link
>
I had the Dillon vibratory polisher. I bought it to deburr aluminum workpieces. It was *way too* gentle for that. It took hours to make very little visible progress. Prolly just fine for putting the final polish on brass, though.
Next time, I will go with a real tumbler. Prolly get an old wood lathe and modify to suit:
formatting link
--Winston
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?