766 fire alarm or door closer from an old warehouse. The grey goo is Woods metal, a low melting point alloy. When it gets hot it melts, the two parts come apart and the wire door retainer they were part of breaks and lets the door swing closed.
The complex shape is because these low melting point alloys are soft and prone to creep, if used as a simple tension or shear link. The shape used here puts the alloy in simple compression over most of it, but there's still enough space to let it separate cleanly when melted.
From rec.woodworking:
#762: Dunno #763: Dunno #764: Baseball bat #765: Looks like a carburetor adjusting tool. #766: Dunno #767: I'd say there is a recess or hole over the top of the tee.
Golf tees taper quite alot. The hole may be a tight fit where the wood meets the tee but really loose at the tip. They also flex. So you could bend it a little or soak the block in water to soften it.
The wood was soaked in water for awhile then compressed in a vise. After the wood dried the tee was inserted. The wood was then placed in water again and expanded back to it's original size.
A leveling jack of some sort - 2 x quick release / set levers, cross bar through bolt head to fine adjust.
Fire alarm or door closer from an old warehouse. (dingbat)
765 is an old points adjusting tool for GM vehicles.
767 ... maybee the golf tee was steambathed. at some high temperature wood can be bent.
formatting link
greetings from germany Chris
I was hoping someone else knew. I still have one (KD) along with a ton of other special tools! Dave
Posted Via Usenet.com Premium Usenet Newsgroup Services
---------------------------------------------------------- ** SPEED ** RETENTION ** COMPLETION ** ANONYMITY **
----------------------------------------------------------
formatting link
I'll guess that there is a space that has been drilled out in the hole in which the tee sits - as though the hole was first drilled at a 45 degree angle, and rotated until it was verticle (in-line with the original hole). The space is hidden by the tee when the tee is in position.
My guesses:
762. Parallel pipe/rod coupler? 763. Quick release jack stand? 764. (Hard to tell without the scale) Tip of a hollowed out baseball bat (I've never seen one)? 765. Carburetor and distributor points adjusting tool (verified with Google search). 766. Object used to connect cables or chains, but keep them electrically isolated? 767. The wood was steamed or soaked in water, compressed, the tee inserted, then the wood expanded (I've made items like this one).Carl G.
It's intriguing, isn't it? It's clearly designed to clamp two round, or roundish, things. If it held them at an angle I'd say it was some sort of picture frame maker or something. But it holds these things parallel
- and fairly precisely.
KD tools.. the expensive ones that GM sends you every year. ;~) Points dwell adjustment tool for the GM caps with the window. The 4 and 6 bangers had to have the cap off with a screwdriver in the a notch in the distributor base for points adjustments. The pictured tool also worked with different attachments to adjust the carbs also.
762, temp cable splice to hook up temp power on sites near bare overhead conductors, or to earth conductors. 763, quick set machinists jack.
#766 will disassemble itself when subjected to excessive heat. Similar items are used in Theatre proscenium fire curtains.
Assuming that's a wooden golf tee there....
It wood not be impossible to create the object from one piece of would by removing all the material which "isn't there" in the finished assembly, right?
I seriously doubt that was how it was done.
Jeff
Most people that I've shown this piece of hardware think it might be some type of connector that was meant to give way under a certain amount of weight or stress, but I like your fire door closer idea. I haven't had any luck searching the web for similar devices, I'm wondering where you've seen one before and if you know any other terms for it.
Thanks, Rob
It's called a fusible link. see, z.b.
scott
Leon, I should send pictures to this guy of some of the (GM/VW/HONDA and others) special tools I have been forced to buy over the last 30 years ;-0
Dave
Posted Via Usenet.com Premium Usenet Newsgroup Services
---------------------------------------------------------- ** SPEED ** RETENTION ** COMPLETION ** ANONYMITY **
----------------------------------------------------------
formatting link
It does appear to be a jack, and you're correct about the quick release levers and the fine adjust on the top. Also, on the top part, that's an arrow pointing to the right but you can't see the lower part of the arrow head. If you turn it around to look at the other side, it also has an arrow head in the same spot pointing right.
formatting link
The seller said that he didn't know what it was until an old timer told him that he recognized it as an old printer's or type setter's tool. I haven't been able to verify if this is true or not. There is some text on the bottom of both sides which reads:
"MORGANS WICOX PATENT"
and
"M & W PAT 4 HICH LOCK", not sure about the HICH.
The text can be seen in this photo:
formatting link
I did find an M & W Printing on the web but I haven't yet found their web site, I might give them a call tomorrow and see how long they've been in business.
Rob
Thanks! Those sites are good references; I think that the one in my photos is probably a fusible link but I'm still going to do a little more research on it.
Rob
Join the Discussion
Have something to add? Share your thoughts — no account required.
Didn't find your answer?
Ask the community — no account required