⚡ Welding Forums

6253 Threads Posts
to

Purox CW-300 Oxy/Acetylene Torch

I have a question. I recently came across the torch head for a Purox CW-300 torch. So I have the part that goes from th...
11 comments posted 22yrs
posted by ringothecat
11 comments posted 22yrs posted by ringothecat

R: welding thin cast iron

I did the exact same repair years ago before I knew better. I only had a little 100v MIG and after a coincidental prehe...
0 comments posted 22yrs
posted by bcarter
0 comments posted 22yrs posted by bcarter

Hobart Handler 140 vs. Lincoln Weld-Pak 3200HD

I'd like to hear from some of you more experienced guys, if you can spare a few minutes, about which of these two machi...
10 comments posted 22yrs
posted by rmorgan7
10 comments posted 22yrs posted by rmorgan7

brazing manifolds to improve seal

I have an old skidsteer which has a three part exhaust/intake manifold. The face of the manifolds are pitted and don't...
3 comments posted 22yrs
posted by bruce
3 comments posted 22yrs posted by bruce

High-tech Metal Finishes

Has anyone tried any of these folk's stuff? Someone mentioned it to me and it looks interesting: http://www.birchwoodcas...
3 comments posted 22yrs
posted by edsusenet
3 comments posted 22yrs posted by edsusenet

Thanks

I just wanted to drop a line to say thanks to all the regular contributors of both RCM and SEJW for sharing their colle...
1 comments posted 22yrs
posted by gjpostmanospam
1 comments posted 22yrs posted by gjpostmanospam

Question on Pipe Welding term

My local newspaper had ad for pipe welder and stated that you should be able to Walk The Cup. What does this term refer...
5 comments posted 22yrs
posted by khenry
5 comments posted 22yrs posted by khenry

TIG Tungsten Size question

What are the consequences of using tungstens that are larger than the minimum size? I commonly use 1/8" for most of my...
4 comments posted 22yrs
posted by WanderingMetalHead
4 comments posted 22yrs posted by WanderingMetalHead

Steel Shot for Positioning

I followed Earnie's advice and bought a bag of shot. It works great for positioning small parts for welding. Has anyone...
2 comments posted 22yrs
posted by edsusenet
2 comments posted 22yrs posted by edsusenet

Hypertherm Powermax 900 views

Anyone any comments on the Hypertherm Powermax 900 plasma cutter? I've been offered a 3 year old one that seems to be i...
0 comments posted 22yrs
posted by andrew
0 comments posted 22yrs posted by andrew

Thermal_Arc MIG

I would like opinions on the Thermal_Arc 251 Fabricator. I've read the sales sheet, it has "features", but I'd like to...
1 comments posted 22yrs
posted by 2regburgess
1 comments posted 22yrs posted by 2regburgess

FS - Oxy/Acy Setup

I have a Oxy/Acy setup I purchased at the local welding supply house (Boggs in Cocoa). I own tanks not rented. Have pap...
0 comments posted 22yrs
posted by rmo7hateallspam
0 comments posted 22yrs posted by rmo7hateallspam

small water cooled mig

are there any small (for tighter work clearance) water cooled mig guns available? have not found one less than 350 amps....
4 comments posted 22yrs
posted by 123
4 comments posted 22yrs posted by 123

Cheap welding machine on Ebay

I saw this really cheap welding machine on Ebay, it's good enough to do smoe simple work? 100 AMP ARC WELDER WELDING MAC...
5 comments posted 22yrs
posted by abc4435
5 comments posted 22yrs posted by abc4435

Beginner advice sought

I am a carpenter. My stick welding experience is limited to occasional small projects usually working on bits of light...
3 comments posted 22yrs
posted by oldblock
3 comments posted 22yrs posted by oldblock