chuck sticking on spindle

I have a lathe with a 2 1/4" threaded spindle with 6 tpi. It came with a 3-jaw but no 4-jaw chuck. I got an 8-inch 4-ja...
10 comments posted 21yrs
posted by notreally
10 comments posted 21yrs posted by notreally

how to make a hole /dogleg tool

This is a newbe question I'm working in aluminium, the origional plans I'm following had a lot of work done on a Lathe...
1 comments posted 21yrs
posted by pbreed
1 comments posted 21yrs posted by pbreed

making a '3 cornered scraper'

I have need of an old tool called a 3 cornered scaper. It is at firs sight, similar to a triangular file, with no teeth...
13 comments posted 21yrs
posted by doc.1vmnln
13 comments posted 21yrs posted by doc.1vmnln

hot wire foam cutter

There *is* some metal in this. I made a quick 'n dirty hot wire foam cutter to make a foam disc for a project. http://us...
2 comments posted 21yrs
posted by dforeman
2 comments posted 21yrs posted by dforeman

OT- Of interest 50 yrs later

http://www.heritage.org/Research/PoliticalPhilosophy/hl619.cfm A scholarly look at the Kerner Commision report and back...
6 comments posted 21yrs
posted by gunner
6 comments posted 21yrs posted by gunner

Machine moving skates

When my mill was delivered the crew used 4 small object that I can only describe as skates. They were made of a steel a...
9 comments posted 21yrs
posted by jdincau
9 comments posted 21yrs posted by jdincau

Working with Invar metal

What precautions should be taken when working with invar low expansion metal. I am told that it is a controlled metal as...
13 comments posted 21yrs
posted by epmajden
13 comments posted 21yrs posted by epmajden

Mounting your angle grinder

I'm looking for schemes for mounting the angle grinder so that I can use it as both a metal saw and a grinder (changing...
6 comments posted 21yrs
posted by mhorowitREMOVE_THESE_CAPS
6 comments posted 21yrs posted by mhorowitREMOVE_THESE_CAPS

Gold Iridite finish for steel?

Hi Group I have some precision STEEL sheet metal parts that need to be made corrosion resistant. I have heard of a gold...
6 comments posted 21yrs
posted by <r.laury
6 comments posted 21yrs posted by <r.laury

Trailer hitch question

I bought a 1-1/4 bolt-on frame hitch receiver, after getting it on I noticed that the hole for the pin that locks the h...
13 comments posted 21yrs
posted by mikepatterson
13 comments posted 21yrs posted by mikepatterson

quick/dirty clamping of vertical rod in tube?

I've seen blacksmiths make forge stock stands using a trick: the stand's vertical member is a tube (e.g. 1/2" pipe) and...
6 comments posted 21yrs
posted by grant
6 comments posted 21yrs posted by grant

OT - burning logs versus wood chips

Is there any difference between burning wood logs versus burning wood chips from a large chipper? It seems like wood ch...
22 comments posted 21yrs
posted by stone75
22 comments posted 21yrs posted by stone75

Sub-MainI in Shop

Several months or so ago there was a thread here I think. Googling etc. to no avail,. Somebody wrote that there was som...
1 comments posted 21yrs
posted by phredd
1 comments posted 21yrs posted by phredd

Bob Cad post processor

Bob Cad post processor I bought Bob Cad version 20 the other day and I cannot seem to get it to translate to the conver...
0 comments posted 21yrs
posted by al.parks
0 comments posted 21yrs posted by al.parks

A sad day

Today I went to fill out a police report. Missing: One Jackson hood with NexGen EQC lens One two horse Sears compressor...
12 comments posted 21yrs
posted by deserttraveler
12 comments posted 21yrs posted by deserttraveler