⏣ General Metalworking

30778 Threads Posts
to

homemade beader / bead-roller?

greets all. i'm looking to 'slap together' a little sheetmetal beader, something to roll simple ribs and offsets. proba...
3 comments posted 22yrs
posted by antoniogatta
3 comments posted 22yrs posted by antoniogatta

Aluminum casting problem

I'm new to this "art" and have searched the Internet for info on my problem but haven't yet found much help so I turn h...
6 comments posted 22yrs
posted by Leon
6 comments posted 22yrs posted by Leon

Ring Roller

I am looking to make a basic ring roller to roll up to 3"x3" square tubing. Can anyone help me on plans for one this si...
2 comments posted 22yrs
posted by sariddle
2 comments posted 22yrs posted by sariddle

Thyratron

KS19699-L4 SOLID STATE THYRATRON 2/68 MFD BY MOTOROLA FOR WESTERN ELECTRIC Still in original box !! Never used !! How c...
6 comments posted 22yrs
posted by md.marino
6 comments posted 22yrs posted by md.marino

For Sale Bridgeport Series 1 CNC mill

$1000 obo. Located in Santa Ana California Unit runs, is complete with all manuals. After an hour or so use, it shuts i...
2 comments posted 22yrs
posted by gunner
2 comments posted 22yrs posted by gunner

OT Gunner's laundry

I have it on good authority that there seems to be some trouble stirring on his clothesline: Jim ======================...
8 comments posted 22yrs
posted by jim_member
8 comments posted 22yrs posted by jim_member

help with compressor!

Hello all, I have an air compressor that blew out the two different O-ring gaskets on the top of the head. One is shape...
12 comments posted 22yrs
posted by poolcuesNOJUNK
12 comments posted 22yrs posted by poolcuesNOJUNK

Resistance soldering

I just finished something similar to the project found here http://www.trainweb.org/bristol-s-gauge/Projects/rsu.html I...
0 comments posted 22yrs
posted by jparkhill
0 comments posted 22yrs posted by jparkhill

Bridgeport project pages updated

I've updated two new photo essays regarding my Bridgeport machine at: http://www.truetex.com/machinery.htm Namely: Movi...
9 comments posted 22yrs
posted by nobody
9 comments posted 22yrs posted by nobody

Texas Anodizing \ Aluminum work?

Anybody out there know of anyone who either does some (aluminum) anodizing, or does fairly inexpensive aluminum welding...
7 comments posted 22yrs
posted by mburggra1
7 comments posted 22yrs posted by mburggra1

OT: Another Use for Laser Pointer(s)

yet more marginal input from the mentally challenged. almost every rcm'r has a laser pointer or instrument of some kind...
4 comments posted 22yrs
posted by lcoe
4 comments posted 22yrs posted by lcoe

Eatin' Pig

I know it's early but I wanna give folks a chance to make summer plans. The first saturday in august, which I think is...
3 comments posted 22yrs
posted by etpm
3 comments posted 22yrs posted by etpm

Aluminum heat treating

Anyone got a good pointer to some aluminum heat treating specs? I'm looking for the sequence to do 6061-T6 The issue is...
3 comments posted 22yrs
posted by spamless
3 comments posted 22yrs posted by spamless

7x12 Homier lathe schematic

Does anyone know of a source for a schematic for the electronics on a Homier 7x12 lathe?It is the unit built around scr...
3 comments posted 22yrs
posted by SAYWAT
3 comments posted 22yrs posted by SAYWAT

etching

I am in the process of making several tools for use on the lathe, and hope to sell some of them at cost, I would like t...
3 comments posted 22yrs
posted by Reyd
3 comments posted 22yrs posted by Reyd